Assessment of the Cracking Problem in Newly Constructed Bridge Decks in Colorado

File Language:
English


Details

  • Creators:
  • Corporate Creators:
  • Corporate Contributors:
  • Subject/TRT Terms:
  • Publication/ Report Number:
  • Resource Type:
  • Geographical Coverage:
  • Edition:
    Final Report
  • Corporate Publisher:
  • Abstract:
    Early age cracking on concrete bridge decks has been experienced by many DOTs. In Colorado the cracking problem on newly constructed bridge decks has not been completely solved. In this study, the extent and causes of the cracking problem were investigated, and necessary changes to alleviate the cracking problem were identified. To achieve these goals, current CDOT practice was reviewed and compared with other DOTs practices for construction of bridge decks. A database analysis of field inspection results was performed. Presently, 18% of newly constructed bridge decks in Colorado have no early cracking problem, and the rest (82 %) have various degrees of cracking problems. The results of the database analysis were then confirmed by field inspections conducted on nine newly constructed bridge decks. An extensive literature review was performed. Past research activities in Colorado were reviewed, current CDOT practices for controlling the bridge deck cracking problem were assessed, and recommendations to alleviate the cracking problem were identified. From the literature survey and previous research studies, the causes of cracking in newly constructed bridges can be categorized as material, design, construction, and environmental factors. High early age shrinkage of concrete is a major contributor among the adverse material factors. The cracking can also be a direct result of several structural design factors. Based on the results of field inspections, the cracks typically form above supporting members, such as girders or piers, and have large and uniform spacing. This is a result of tensile stresses from negative bending moments in the deck above supports. The construction and environmental factors (such as wind speed, temperature, and curing procedures) greatly affect the shrinkage of the concrete. Due to very limited information regarding deck curing or placement conditions, it has not been possible to determine the specific impact of these factors on early age deck cracking of the inspected bridges.
  • Format:
    PDF
  • Download URL:
  • File Type:
    Filetype[PDF - 1.98 MB]
  • Collection(s):
  • Main Document Checksum:
    urn:sha-512:630c3742603a4992a323a3b4b0c3ad1d52868e56bce07ac0a820e1007c5b5fa1b9b50cc9770a00c34dbb4ec5c5b9015f4a5dcc0128902163660be5ddcc66e57c
File Language:
English
ON THIS PAGE
 Found an issue?
Send us an email at:
ROSA P serves as an archival repository of USDOT-published products including scientific findings, journal articles, guidelines, recommendations, or other information authored or co-authored by USDOT or funded partners. As a repository, ROSA P retains documents in their original published format to ensure public access to scientific information.