Advanced Search
Select up to three search categories and corresponding keywords using the fields to the right. Refer to the Help section for more detailed instructions.

Search our Collections & Repository

For very narrow results

When looking for a specific result

Best used for discovery & interchangable words

Recommended to be used in conjunction with other fields

Dates

to

Document Data
Library
People
Clear All
Clear All

For additional assistance using the Custom Query please check out our Help Page

i

Polymer impregnated bridge slabs : interim report.

Filetype[PDF-1.68 MB]


English

Details:

  • Creators:
  • Subject/TRT Terms:
  • Publication/ Report Number:
  • Resource Type:
  • Geographical Coverage:
  • Corporate Publisher:
  • Abstract:
    The procedure used for producing precast slabs of polymer impregnated concrete (PIC) and described in this report was generally satisfactory from an operational standpoint. A strength loss of 14%, attributable to the drying step, was observed in PIC cylinders; however, residual strengths for this class of concrete were satisfactory. The freeze-thaw durability of PIC specimens was essentially the same as the excellent performance exhibited by the control concrete. The average maximum depth of polymer impregnation observed in cores from the slabs was 1.0 in. (25 mm). The impregnated zone was found to contain a series of discontinuous microcracks resulting from the polymer treatment. These cracks allowed CI-penetrations at a depth of 0.8 in. (19 mm) that equaled or exceeded those at this depth in the control concrete. Additional research with experimental slabs is recommended with the objective of eliminating the microcracking associated with the impregnated zone.
  • Format:
  • Collection(s):
  • Main Document Checksum:
  • Download URL:
  • File Type:

Supporting Files

  • No Additional Files
More +

You May Also Like

Checkout today's featured content at rosap.ntl.bts.gov